Sure, just keep in mind when you make your nital that and look for the
99.99% pure alcohol that even concentrated nitric acid is 30% water
(same as the low grade isopropanol from the supermarket).


-----Original Message-----
From: Craig Moody <meteoritesnorth at hotmail.ca>
To: MetList <meteorite-list at meteoritecentral.com>
Sent: Thu, Jan 26, 2012 7:34 pm
Subject: [meteorite-list] Etching solution



Hello all.

I am going to perform my first etch, of a Sikhote-Alin slice with
Nitol, but I
was wondering if Isopropyl can be substituted for the Ethanol? Any
advise would
be apreciated.

Thanks
Craig
______________________________________________

Visit the Archives at
http://www.meteoritecentral.com/mailing-list-archives.html
Meteorite-list mailing list
Meteorite-list at meteoritecentral.com
http://six.pairlist.net/mailman/listinfo/meteorite-list
Received on Thu 26 Jan 2012 09:37:11 PM PST


Help support this free mailing list:



StumbleUpon
del.icio.us
reddit
Yahoo MyWeb